Walther Trowal MV 21 vs MV 25 vibratory finishing catalog comparison

Review MV 21 and MV 25 from the official Walther Trowal MV brochure marked 12/20, physical PDF page4. Filter 7 source fields and record your part, fixture or separation, site and acceptance questions before downloading the current review. Volume and drive entries retain their printed physical bases. The captured current web table is separate from the versioned PDF and does not establish an offered machine.

Walther Trowal MV 21 vs MV 25 vibratory finishing catalog comparison - usable-volume-review diagram - Jintaijin
Original source-data diagram; Walther Trowal 12/20, physical PDF page4. No actual trial or current configuration approval.

Compare catalog fields and record configuration questions

Choose a source field group; optionally record your own review requirements.

Versioned catalog rows

Source fieldMV 21MV 25
Machine weight, empty (kg; printed qualifier retained)ca. 895ca. 1,145
Power requirements (kVA; not kW)3.55.0
Batch load - ceramic media (kg; not part load)230470
Batch load - plastic media (kg; not part load)150310
Usable volume (L; not part batch load)130260
Max. workpiece dimension measured diagonally (mm)ca. 570ca. 700
Max. motor speed (rpm; inverter adjustable, not setpoint)3,0003,000

Separate usable volume from part batch load

The 12/20 PDF lists MV 21 with 130 L usable volume and MV 25 with 260 L. Neither number establishes a part-only load, cycle time, production rate or approved operating fill. Review the actual part arrangement, media grade and media-to-parts occupancy with the trial owner. Ceramic-media batch loads are 230 kg and 470 kg; plastic-media batch loads are 150 kg and 310 kg. These kg entries belong to media types and must not be converted into workpiece load or transferable density. The brochure describes workpieces clamped at the bowl bottom, with mechanical or electromagnetic clamping systems requiring an actual fixture review.

Review configuration and geometry bases

The empty-weight entries are ca. 895 kg for MV 21 and ca. 1,145 kg for MV 25. The printed qualifiers are retained; MV32 is written a.3,330 in this version, so no correction to a different qualifier or current weight is made. Maximum workpiece dimensions are measured diagonally and printed ca. 570 mm and ca. 700 mm. A single diagonal cannot approve the clamping interface, electromagnetic suitability, media access, local rib protection, transport loading or floor support. Lettered drawing dimensions are excluded from this tool.

Walther Trowal MV 21 vs MV 25 vibratory finishing catalog comparison - configuration-basis-review diagram - Jintaijin
Original source-data diagram; Walther Trowal 12/20, physical PDF page4. No actual trial or current configuration approval.

Keep drive units and speed statements separate

Power requirements are 3.5 kVA for MV 21 and 5.0 kVA for MV 25. This is an apparent-power row, distinct from current-web kW at specified motor speeds. No power factor or conversion is provided. The maximum motor-speed entries are 3,000 rpm and 3,000 rpm with infinitely adjustable frequency inverter in the brochure footnote. These maxima are not validated processing setpoints. No total connected load, energy consumption, electricity cost, cycle time or finishing result is calculated.

Walther Trowal MV 21 vs MV 25 vibratory finishing catalog comparison - drive-version-review diagram - Jintaijin
Original source-data diagram; Walther Trowal 12/20, physical PDF page4. No actual trial or current configuration approval.

Confirm the actual version and installed options

The PDF contains MV21, MV25 and MV32 columns only. The current website also lists MV50; this does not provide an MV50 record in the versioned brochure and no MV50 pair is generated here. Clamping configuration, pneumatic media discharge and installed automation require the actual offered drawing. Narrative references to medical or aerospace parts are not qualification or performance evidence for your part.

Keep current-web differences visible

MV 25: weight is ca. 1,145 in the PDF and approx. 1,250 under current web label "Unladen weight (kg)". MV 25: ceramic is 470 in the PDF and 450 under current web label "Ceramic grinding media capacity (kg)". MV 25: plastic is 310 in the PDF and 300 under current web label "Plastic abrasive media capacity (kg)". MV 25: usable is 260 in the PDF and 250 under current web label "Max. usable volume (l)". PDF kVA and current-web kW rows have different physical bases; no conversion or numeric equivalence. PDF MV32 empty weight is printed a.3,330; preserve the atypical qualifier, do not silently correct to ca. Current web includes MV50; this PDF has no MV50 parameter record and no pair is created for it. Keep versions and physical bases separate and request the actual offered specification.

Official current MV product page, captured2026-10-05. Selected numeric rows were compared; this is not an exhaustive reconciliation of drawings, options, physical power bases or offered configurations.

Source and scope

Official MV brochure, 12/20, physical page4; captured2026-10-05. Independent Walther Trowal reference. No Jintaijin supply, partnership, equivalent machine, actual finishing result, medical/aerospace qualification or current offer is established. User notes are USER_RECORDED_NOT_VERIFIED. Diagrams are original source-data references, not product photos or customer evidence.

Questions about this pair

How do MV 21 and MV 25 compare in usable volume?

The 12/20 PDF lists MV 21 with 130 L usable volume and MV 25 with 260 L. Neither number establishes a part-only load, cycle time, production rate or approved operating fill. Review the actual part arrangement, media grade and media-to-parts occupancy with the trial owner. Ceramic-media batch loads are 230 kg and 470 kg; plastic-media batch loads are 150 kg and 310 kg. These kg entries belong to media types and must not be converted into workpiece load or transferable density. The brochure describes workpieces clamped at the bowl bottom, with mechanical or electromagnetic clamping systems requiring an actual fixture review.

What configuration or geometry fields need confirmation?

The empty-weight entries are ca. 895 kg for MV 21 and ca. 1,145 kg for MV 25. The printed qualifiers are retained; MV32 is written a.3,330 in this version, so no correction to a different qualifier or current weight is made. Maximum workpiece dimensions are measured diagonally and printed ca. 570 mm and ca. 700 mm. A single diagonal cannot approve the clamping interface, electromagnetic suitability, media access, local rib protection, transport loading or floor support. Lettered drawing dimensions are excluded from this tool.

Can these drive rows be used as power or process settings?

Power requirements are 3.5 kVA for MV 21 and 5.0 kVA for MV 25. This is an apparent-power row, distinct from current-web kW at specified motor speeds. No power factor or conversion is provided. The maximum motor-speed entries are 3,000 rpm and 3,000 rpm with infinitely adjustable frequency inverter in the brochure footnote. These maxima are not validated processing setpoints. No total connected load, energy consumption, electricity cost, cycle time or finishing result is calculated.

Which version and availability statements must remain separate?

The PDF contains MV21, MV25 and MV32 columns only. The current website also lists MV50; this does not provide an MV50 record in the versioned brochure and no MV50 pair is generated here. Clamping configuration, pneumatic media discharge and installed automation require the actual offered drawing. Narrative references to medical or aerospace parts are not qualification or performance evidence for your part.

Does the current official website agree with the PDF?

MV 25: weight is ca. 1,145 in the PDF and approx. 1,250 under current web label "Unladen weight (kg)". MV 25: ceramic is 470 in the PDF and 450 under current web label "Ceramic grinding media capacity (kg)". MV 25: plastic is 310 in the PDF and 300 under current web label "Plastic abrasive media capacity (kg)". MV 25: usable is 260 in the PDF and 250 under current web label "Max. usable volume (l)". PDF kVA and current-web kW rows have different physical bases; no conversion or numeric equivalence. PDF MV32 empty weight is printed a.3,330; preserve the atypical qualifier, do not silently correct to ca. Current web includes MV50; this PDF has no MV50 parameter record and no pair is created for it. Keep versions and physical bases separate and request the actual offered specification.

Related review tools

Prepare a sample review enquiry

For SurfacePolish equipment discussions, provide your part drawing, finishing objective, fixture and media restrictions, and acceptance method. This reference does not confirm third-party machine supply.

Open the SurfacePolish enquiry form

#+86-592-2381506

Email : info@surface-polish.com

Headquarters address : No. 31, Xinchang Road, Xinyang Industrial Zone, Haicang District, Xiamen

click here to leave a message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Preparing secure enquiry form…

Home

Products

whatsapp

contact