Alumina Porcelain (Ball)

This page reproduces the published catalog rows for Alumina Porcelain (Ball) exactly as they appear on 5 Jintaijin product pages, and shows where those pages disagree with each other. The specification string, shape and bullet markers are source values. They are not a measured removal rate, a gloss figure, a cycle time or a supply guarantee.

Alumina Porcelain (Ball) - published specification - Jintaijin
Published Specification. Original graphic built from published catalog cells; not a measured result.

Check the published rows and prepare a supplier review

Select a source page, notation or marker, then check the published rows.

Published catalog rows for Alumina Porcelain (Ball)

Specification (as published)Shapep39p43p44p48p49
Alumina Porcelain (Ball)2、4、6、8、10、12、15、20
Single values separated by the ideographic comma
BallF+FFF+FFF+FFno markerno marker

Function columns: VR, R, N, NF, M, MF, F, FF. Blank means no marker on that page.

Alumina Porcelain (Ball) - source marker comparison - Jintaijin
Source Marker Comparison. Original graphic built from published catalog cells; not a measured result.
Alumina Porcelain (Ball) - supplier and sample review - Jintaijin
Supplier And Sample Review. Original graphic built from published catalog cells; not a measured result.

What the published rows actually say

The table below is a transcription of the published cells. Specification strings are reproduced character for character, including the ideographic comma separators used on the pages. Where a source cell is empty it is shown as empty rather than filled from another page.

The Function columns use a bullet marker. It is an original qualitative manufacturer marker. It does not state a removal rate, a gloss value, a multiplier or a duration, and this page does not convert it into one.

The same product is marked differently on different pages

For this product the bullet markers are not identical across the Jintaijin pages that list it. The table shows the markers exactly as each page publishes them. No page is treated as authoritative over another, no majority vote is taken and no average is computed.

That disagreement is itself useful procurement information: before you compare grades, ask the supplier which page reflects the current product. A buyer who assumed the catalog is internally consistent could otherwise plan a trial against a marker that another page does not support.

Before you run a trial

A catalog cell does not approve a workpiece. Confirm the current grade, particle geometry and machine compatibility with the supplier. For small holes, slots or recesses, establish how media enters, whether it can lodge and how it is removed. For pastes or powders, obtain the current safety data and preparation procedure. Then define the acceptance method and the sample identity before the trial starts.

Source pages and what they disagree about

Recorded source conditions

Rows were reconstructed from the published rowspan and colspan grid and verified against an independent re-parse of the same pages. Specification strings, shapes and markers are reproduced without correction, conversion or averaging.

Frequently asked questions

What does the bullet marker in the Function column mean?

It is an original qualitative marker used by the manufacturer to group a product under function headings such as VR, R, N, NF, M, MF, F or FF. The page does not treat it as a removal rate, gloss value, multiplier or cycle time, and no such value can be derived from it.

Why does this page show different markers for the same product on different Jintaijin pages?

Because the published pages disagree. Both readings are reproduced side by side and neither is treated as authoritative. No average, score or corrected value is computed.

Are the # numbers millimetres?

No. The column header reads Specification (mm) but rows written with the # symbol use a mesh or grit designation. They are preserved exactly and are not converted to a length.

Does an empty specification cell mean no size is available?

No. It means the published row does not state a specification in that cell. It is not evidence for or against any available size.

Does this page recommend a grade or a process?

No. It reproduces published catalog values and discloses their inconsistencies. Grade selection, machine compatibility, loading and finishing time remain decisions for a trial with the supplier.

Related tools

Discuss your media requirements

Open the Jintaijin inquiry page

#+86-592-2381506

Email : info@surface-polish.com

Headquarters address : No. 31, Xinchang Road, Xinyang Industrial Zone, Haicang District, Xiamen

click here to leave a message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Preparing secure enquiry form…

Home

Products

whatsapp

contact