Rosler ceramic RXF vs RX media composition and catalog size matrix comparison
Compare Rosler ceramic RXF and RX from the 07/2023 US.338.27 brochure. Approximate bulk density is printed as 103 and 102 lbs/ft3, respectively. Query a source shape and printed unit to inspect each original list. Millimeter and inch cells remain independent nominal strings, and blanks do not establish unavailable supply. Record current specification, separation and sample-review questions without treating this catalog as part-fit approval.
Query source shapes and independent unit lists
Original composition and shape/unit cells
| Source field | RXF | RX |
|---|---|---|
| Approximate bulk density | 103 lbs/ft3 | 102 lbs/ft3 |
| Triangle Straight Cut / mm | D: 06/06 | 10/10 | 15/10 | 15/15 | D: 04/04 | 05/05 | 10/10 |
| Triangle Straight Cut / in | SCT: 1/4 x 1/4 | 3/8 x 3/8 | 5/8 x 3/8 | 3/8 x 3/8 | SCT: 5/32 x 5/32 | 3/16 x 3/16 | 3/8 x 3/8 |
| Triangle Rounded / mm | F: No entry printed; current supply not established. | F: 15/15 | 20/20 |
| Triangle Rounded / in | T: No entry printed; current supply not established. | T: 5/8 x 5/8 | 3/4 x 3/4 |
| Triangle Angle Cut / mm | S: 06/06 | 10/06 | 10/15 | 15/18 | S: 06/10 | 08/08 | 10/15 | 15/15 | 20/10 | 20/20 | 25/25 | 30/12 | 40/15 | 40/20 |
| Triangle Angle Cut / in | ACT: 1/4 x 1/4 | 3/8 x 1/4 | 3/8 x 5/8 | 5/8 x 3/4 | ACT: 1/4 x 3/8 | 5/16 x 5/16 | 3/8 x 5/8 | 5/8 x 5/8 | 3/4 x 3/8 | 3/4 x 3/4 | 1 x 1 | 1-1/8 x 1/2 | 1-5/8 x 5/8 | 1-5/8 x 3/4 |
| Cylinder Straight Cut / mm | Z: No entry printed; current supply not established. | Z: 06/12 |
| Cylinder Straight Cut / in | SCC: No entry printed; current supply not established. | SCC: 1/4 x 1/2 |
| Cylinder Angle Cut / mm | ZC: 05/10 | 08/15 | ZC: 03/05 | 05/08 | 07/15 | 08/15 | 10/20 | 12/25 | 15/20 | 22/40 | 30/40 |
| Cylinder Angle Cut / in | ACC: 3/16 x 3/8 | 5/16 x 5/8 | ACC: 1/8 x 3/16 | 3/16 x 5/16 | 9/32 x 5/8 | 5/16 x 5/8 | 3/8 x 3/4 | 1/2 x 1 | 5/8 x 3/4 | 7/8 x 1-5/8 | 1-1/8 x 1-5/8 |
| Tri Cyl / mm | QZ: 08 | QZ: 10 | 12.5 | 15 | 25 | 38 |
| Tri Cyl / in | TC: 5/16 | TC: 3/8 | 1/2 | 5/8 | 1 | 1-1/2 |
| Ellipse Straight Cut / mm | E: 08/09/03 | E: No entry printed; current supply not established. |
| Ellipse Straight Cut / in | SCE: 5/16 x 11/32 x 1/8 | SCE: No entry printed; current supply not established. |
| Ellipse Angle Cut / mm | ES: 15/22/06 | ES: No entry printed; current supply not established. |
| Ellipse Angle Cut / in | ACE: 5/8 x 7/8 x 1/4 | ACE: No entry printed; current supply not established. |
| Tristar Straight Cut / mm | DZ: No entry printed; current supply not established. | DZ: 04/04 | 06/06 | 10/10 |
| Tristar Straight Cut / in | SCTRI: No entry printed; current supply not established. | SCTRI: 5/32 x 5/32 | 1/4 x 1/4 | 3/8 x 3/8 |
| Tristar Angle Cut / mm | DZS: 10/12 | 15/06 | DZS: No entry printed; current supply not established. |
| Tristar Angle Cut / in | ACTRI: 3/8 x 1/2 | 5/8 x 1/4 | ACTRI: No entry printed; current supply not established. |
| Arrowhead / mm | W: No entry printed; current supply not established. | W: No entry printed; current supply not established. |
| Arrowhead / in | ARR: No entry printed; current supply not established. | ARR: No entry printed; current supply not established. |
| Pyramid Tetrahedron / mm | P: No entry printed; current supply not established. | P: No entry printed; current supply not established. |
| Pyramid Tetrahedron / in | TET: No entry printed; current supply not established. | TET: No entry printed; current supply not established. |
| Cone / mm | K: No entry printed; current supply not established. | K: No entry printed; current supply not established. |
| Cone / in | CN: No entry printed; current supply not established. | CN: No entry printed; current supply not established. |
| Balls / mm | G: No entry printed; current supply not established. | G: No entry printed; current supply not established. |
| Balls / in | BLS: No entry printed; current supply not established. | BLS: No entry printed; current supply not established. |
Source interpretation for this pair
- RXF: Graphical grinding traces are not numerical rankings.
- RXF: Metric and imperial cells are retained independently; no conversion or positional pairing.
- RXF: Blank cells mean no printed entry in this captured matrix, not unavailable supply.
- RXF: Printed punctuation, missing separators and apparent metric/imperial discrepancies are preserved without correction.
- RXF: The last imperial Triangle Straight Cut entry is printed 3/8 x 3/8 alongside metric entries ending 15/15; no correction or equivalence is assumed.
- RX: Graphical grinding traces are not numerical rankings.
- RX: Metric and imperial cells are retained independently; no conversion or positional pairing.
- RX: Blank cells mean no printed entry in this captured matrix, not unavailable supply.
- RX: Printed punctuation, missing separators and apparent metric/imperial discrepancies are preserved without correction.
- 07/2023 US.338.27 historical reference; specifications subject to change.
- Approximate bulk density is not material true density or a process result.
- Nominal millimeter and inch entries remain independent printed lists; no conversion or stock approval.
- Metric cylinder-angle-cut code is ZS on physical page6 and ZC on physical page7; page-specific values are retained.
- RMB/D1 vs RMD/D1 and WHPC vs WPHC name conflicts are excluded from this comparison dataset.
- Asterisk, punctuation and apparent discrepancies are retained without inferred correction.
Source and current sample scope
Official Rosler Consumables brochure, US.338.27, 07/2023; physical matrix pages 6,7. Captured and hash verified 2026-10-05.
This independent Rosler historical reference supports a current supplier and sample discussion. It does not establish Jintaijin supply, partnership, equivalent media, current availability or a successful trial. Request a current dimensioned specification and check the real part, separation method and wear condition. Your records remain unverified.
Questions about this pair
What does this composition comparison show?
RXF and RX have approximate bulk-density entries of 103 and 102 lbs/ft3. Their original shape/unit cells appear separately below; density is not a cutting-performance rating.
Does a blank cell mean that a product is unavailable?
It means no entry is printed in this captured matrix. Ask the supplier about current specifications and availability.
Can the millimeter and inch lists be converted or paired?
These nominal printed lists are retained independently. Apparent discrepancies and punctuation are preserved. The tool does not pair entries by position or calculate a conversion.
Does this tool recommend a finishing recipe or approve a part opening?
No. There is no validated input linking this historical table to a particular part, process, wear state or acceptance criterion. Record sample and separation checks with a current supplier.
What source details need confirmation?
Graphical grinding traces are not numerical rankings. Metric and imperial cells are retained independently; no conversion or positional pairing. Blank cells mean no printed entry in this captured matrix, not unavailable supply. Printed punctuation, missing separators and apparent metric/imperial discrepancies are preserved without correction. The last imperial Triangle Straight Cut entry is printed 3/8 x 3/8 alongside metric entries ending 15/15; no correction or equivalence is assumed. Graphical grinding traces are not numerical rankings. Metric and imperial cells are retained independently; no conversion or positional pairing. Blank cells mean no printed entry in this captured matrix, not unavailable supply. Printed punctuation, missing separators and apparent metric/imperial discrepancies are preserved without correction. This independent Rosler historical reference supports a current supplier and sample discussion. It does not establish Jintaijin supply, partnership, equivalent media, current availability or a successful trial. Request a current dimensioned specification and check the real part, separation method and wear condition. Your records remain unverified.
Related review tools
Prepare a sample review
Provide the current media specification, part drawing and acceptance method for a SurfacePolish discussion.
Open the SurfacePolish enquiry form