Rosler plastic PFC-ZF vs PFC-AF media composition and catalog size matrix comparison
Compare Rosler plastic PFC-ZF and PFC-AF from the 07/2023 US.338.27 brochure. Approximate bulk density is printed as 86 and 75 lbs/ft3, respectively. Query a source shape and printed unit to inspect each original list. Millimeter and inch cells remain independent nominal strings, and blanks do not establish unavailable supply. Record current specification, separation and sample-review questions without treating this catalog as part-fit approval.
Query source shapes and independent unit lists
Original composition and shape/unit cells
| Source field | PFC-ZF | PFC-AF |
|---|---|---|
| Approximate bulk density | 86 lbs/ft3 | 75 lbs/ft3 |
| Cone Taper Top / mm | K: 10 | 16 | K: 10 | 16 |
| Cone Taper Top / in | CN: 3/8 | 5/8 | CN: 3/8 | 5/8 |
| Cone Round Top / mm | KR: 20 | 25 | KR: 14 | 19 |
| Cone Round Top / in | RTC: 3/4 | 1 | RTC: 9/16 | 3/4 |
| Pyramid Tetrahedron / mm | P: 20 | 25 | P: 10 | 20 |
| Pyramid Tetrahedron / in | TET: 3/4 | 1 | TET: 3/8 | 3/4 |
| Pyramid Square Base / mm | PQ: No entry printed; current supply not established. | PQ: 10 |
| Pyramid Square Base / in | PY SQ: No entry printed; current supply not established. | PY SQ: 3/8 |
| Pyramid Diamond Base / mm | PD: No entry printed; current supply not established. | PD: No entry printed; current supply not established. |
| Pyramid Diamond Base / in | PY DI: No entry printed; current supply not established. | PY DI: No entry printed; current supply not established. |
| Triangle / mm | D: No entry printed; current supply not established. | D: No entry printed; current supply not established. |
| Triangle / in | T: No entry printed; current supply not established. | T: No entry printed; current supply not established. |
| Wedge Bowtie / mm | DK: No entry printed; current supply not established. | DK: No entry printed; current supply not established. |
| Wedge Bowtie / in | WDG: No entry printed; current supply not established. | WDG: No entry printed; current supply not established. |
| Tricyl / mm | QZ: No entry printed; current supply not established. | QZ: No entry printed; current supply not established. |
| Tricyl / in | TC: No entry printed; current supply not established. | TC: No entry printed; current supply not established. |
| Tristar / mm | DZ: No entry printed; current supply not established. | DZ: No entry printed; current supply not established. |
| Tristar / in | ST: No entry printed; current supply not established. | ST: No entry printed; current supply not established. |
Source interpretation for this pair
- PFC-ZF: Graphical grinding traces are not numerical rankings.
- PFC-ZF: Metric and imperial cells are retained independently; no conversion or positional pairing.
- PFC-ZF: Blank cells mean no printed entry in this captured matrix, not unavailable supply.
- PFC-ZF: Printed punctuation, missing separators and apparent metric/imperial discrepancies are preserved without correction.
- PFC-AF: Graphical grinding traces are not numerical rankings.
- PFC-AF: Metric and imperial cells are retained independently; no conversion or positional pairing.
- PFC-AF: Blank cells mean no printed entry in this captured matrix, not unavailable supply.
- PFC-AF: Printed punctuation, missing separators and apparent metric/imperial discrepancies are preserved without correction.
- 07/2023 US.338.27 historical reference; specifications subject to change.
- Approximate bulk density is not material true density or a process result.
- Nominal millimeter and inch entries remain independent printed lists; no conversion or stock approval.
- Metric cylinder-angle-cut code is ZS on physical page6 and ZC on physical page7; page-specific values are retained.
- RMB/D1 vs RMD/D1 and WHPC vs WPHC name conflicts are excluded from this comparison dataset.
- Asterisk, punctuation and apparent discrepancies are retained without inferred correction.
Source and current sample scope
Official Rosler Consumables brochure, US.338.27, 07/2023; physical matrix pages 9. Captured and hash verified 2026-10-05.
This independent Rosler historical reference supports a current supplier and sample discussion. It does not establish Jintaijin supply, partnership, equivalent media, current availability or a successful trial. Request a current dimensioned specification and check the real part, separation method and wear condition. Your records remain unverified.
Questions about this pair
What does this composition comparison show?
PFC-ZF and PFC-AF have approximate bulk-density entries of 86 and 75 lbs/ft3. Their original shape/unit cells appear separately below; density is not a cutting-performance rating.
Does a blank cell mean that a product is unavailable?
It means no entry is printed in this captured matrix. Ask the supplier about current specifications and availability.
Can the millimeter and inch lists be converted or paired?
These nominal printed lists are retained independently. Apparent discrepancies and punctuation are preserved. The tool does not pair entries by position or calculate a conversion.
Does this tool recommend a finishing recipe or approve a part opening?
No. There is no validated input linking this historical table to a particular part, process, wear state or acceptance criterion. Record sample and separation checks with a current supplier.
What source details need confirmation?
Graphical grinding traces are not numerical rankings. Metric and imperial cells are retained independently; no conversion or positional pairing. Blank cells mean no printed entry in this captured matrix, not unavailable supply. Printed punctuation, missing separators and apparent metric/imperial discrepancies are preserved without correction. Graphical grinding traces are not numerical rankings. Metric and imperial cells are retained independently; no conversion or positional pairing. Blank cells mean no printed entry in this captured matrix, not unavailable supply. Printed punctuation, missing separators and apparent metric/imperial discrepancies are preserved without correction. This independent Rosler historical reference supports a current supplier and sample discussion. It does not establish Jintaijin supply, partnership, equivalent media, current availability or a successful trial. Request a current dimensioned specification and check the real part, separation method and wear condition. Your records remain unverified.