Compare R 1000.1 BT and R 2000.1 BT from the Roesler dryer factsheet, physical page 2, revision 04/2023. Read the exact source labels, original ratings and options side by side. Choose one of two catalog-field profiles, enter optional maxima in millimetres and export the current comparison for supplier review. Use current drawings and workpiece trials to confirm the offered configuration and drying process.
Compare exact models and original source fields
| Factsheet field | R 1000.1 BT | R 2000.1 BT |
|---|---|---|
| Belt length (mm) | 2,265 mm | 3,765 mm |
| Length of drying tunnel (mm) | 1,000 mm | 2,000 mm |
| Machine width (mm) | 1,000 mm | 1,000 mm |
| Machine height (mm) | 1,325 mm | 1,325 mm |
| Belt width (mm) | 600 mm | 600 mm |
| Loading heigth (mm) | 820 mm | 820 mm |
| F | 500 [unit not explicit / notation retained] | 500 [unit not explicit / notation retained] |
| Length loading area (mm) | 500 mm | 1,000 mm |
| Length output area (mm) | 500 mm | 500 mm |
| J – (mm) | 725 mm | 725 mm |
| Flow height (standard) (mm) | 200 mm | 250 mm |
| L – (mm) | 1,200 mm | 1,200 mm |
| Adjustable heat output (kW) | 22.5 kW | 22.5 kW |
| Total connected load (kW) | 25.5 kW | 25.5 kW |
| Rate of air circulation up to (m³/h) | 3,000 m³/h | 3,000 m³/h |
Adjustable heat output (kW): 22.5 kW versus 22.5 kW; Total connected load (kW): 25.5 kW versus 25.5 kW; Rate of air circulation up to (m³/h): 3,000 m³/h versus 3,000 m³/h.
The complete source table is shown with its original labels and notation. Unit-ambiguous fields, stages, ranges and unselected options remain raw; the query only screens cleared numeric dimension fields.
Compare your catalog-field maxima
Select a profile to see the three exact field names. Leave all three inputs blank for comparison, or enter all three positive decimal maxima in mm. Switching profiles clears previous values so one condition cannot inherit another condition’s limits.
Review the two field conditions separately
For external table, Belt length (mm) is 2,265 mm versus 3,765 mm; Machine width (mm) is 1,000 mm versus 1,000 mm; Machine height (mm) is 1,325 mm versus 1,325 mm. These named fields are compared independently; they do not prove installation clearance, part fit or drying suitability.
For drying passage, Length of drying tunnel (mm) is 1,000 mm versus 2,000 mm; Belt width (mm) is 600 mm versus 600 mm; Flow height (standard) (mm) is 200 mm versus 250 mm. These named fields are compared independently; they do not prove installation clearance, part fit or drying suitability.
Every result names its selected fields and retains the original source record. A field maximum is a numerical query on a catalog value. In particular, aperture and passage values do not constitute maximum permissible workpiece geometry. Consult the drawing and a trial with actual parts, drying media and loading arrangements.
- Belt length and drying-tunnel length are separate fields, not interchangeable installation dimensions.
- 700/800 mm belt widths are available on request only for the *1 records; this dataset retains standard 600 mm.
- Adjustable heat-output ranges remain raw; total connected load is a separate rating, not measured energy consumption.
- Air circulation is catalog air flow, not workpiece throughput.
- The factsheet F row does not state a unit; brochure F-(mm) corroborates a unit, retained as context rather than changing the primary label.
Prepare a supplier review and sample trial
Review the required drying passage independently from the external table. Ask for belt speed, residence-time trials, wet-part carryover and offered belt width. The 700/800 mm alternatives are request options on the marked models, not selected values. Neither air flow nor connected load determines parts per hour.
Record the incoming moisture condition, workpiece geometry, material, sensitivity, handling and separation criteria before requesting a trial. Ask for measured drying outcomes and cycle or residence conditions for the offered setup. This catalog record does not establish acceptable residual moisture, finish quality, corrosion behavior, production output or utility consumption.
Source: Roesler dryer factsheet, physical page 2, revision04/2023. The EN.148.19 revision04/2023 dryer brochure, physical page 7, supplies drawing and label context from the same publisher.
Confirm current configuration, options and availability with the manufacturer. No Jintaijin equivalence or manufacturer partnership is established.
Questions about this pair
What source fields differ between R 1000.1 BT and R 2000.1 BT?
For external table, Belt length (mm) is 2,265 mm versus 3,765 mm; Machine width (mm) is 1,000 mm versus 1,000 mm; Machine height (mm) is 1,325 mm versus 1,325 mm. These named fields are compared independently; they do not prove installation clearance, part fit or drying suitability. Adjustable heat output (kW): 22.5 kW versus 22.5 kW; Total connected load (kW): 25.5 kW versus 25.5 kW; Rate of air circulation up to (m³/h): 3,000 m³/h versus 3,000 m³/h.
Which second field profile is available?
For drying passage, Length of drying tunnel (mm) is 1,000 mm versus 2,000 mm; Belt width (mm) is 600 mm versus 600 mm; Flow height (standard) (mm) is 200 mm versus 250 mm. These named fields are compared independently; they do not prove installation clearance, part fit or drying suitability.
Can these dryer ratings establish throughput or operating cost?
Review the required drying passage independently from the external table. Ask for belt speed, residence-time trials, wet-part carryover and offered belt width. The 700/800 mm alternatives are request options on the marked models, not selected values. Neither air flow nor connected load determines parts per hour. Catalog powers are ratings, not measured consumption. No selected heat stage, cycle time, kg/hour or output guarantee is calculated.
What does a passing maximum-field test mean?
It means each of the three selected source fields is at or below the maximum you entered for that named field. These are independent catalog queries, including aperture or loading fields where selected. They do not establish that a part fits, a dryer fits an installation space or a process will work. Leave all three inputs blank for a comparison, or enter all three positive decimal maxima. Confirm the source revision, offered options, clearance, workpiece handling and sample-trial requirements with the supplier.
Related trial and inspection tools
Discuss your workpiece and sample-trial requirements with Jintaijin