Jintaijin | Independent versioned catalog reference
Roesler TS-30 R 500/800 vs R 500/1000: catalog comparison
Compare R 500/800 and R 500/1000 in the Roesler TS-30 factsheet, physical page 2, revision 05/2024. Inspect work-bowl volume, drawing dimensions and the original drive-power notation. Enter your own volume minimum and machine dimension maxima, then download the current comparison. Confirm actual configuration, drawings and workpiece loading with the supplier before selecting equipment.
Source table and volume basis
| Source field | R 500/800 | R 500/1000 |
|---|---|---|
| Work-bowl volume (profile not specified in volume column) | 210 L | 260 L |
| A: work-bowl width | 500 mm | 500 mm |
| B: work-bowl height | 580 mm | 580 mm |
| C: work-bowl length | 800 mm | 1000 mm |
| D: complete-machine total length | 2355 mm | 2590 mm |
| E: complete-machine total width | 715 mm | 715 mm |
| F: machine height | 1130 mm | 1020 mm |
| Type B work-bowl volume (only if explicitly listed) | Not listed | Not listed |
| A1 source dimension (raw; mm when listed) | NOT_LISTED | NOT_LISTED |
| Drive power (original entry, kW) | 2 x 4,0 | 2 x 4,0 |
| Drive speed (source heading) | 3000 rpm | 3000 rpm |
The TS-30 table lists 210 L for R 500/800 and 260 L for R 500/1000, a right-minus-left difference of 50 L. The basis is work-bowl volume (profile not specified in volume column). These values are not permissible part loads, batch weights or throughput. Type B volume is not listed for both models; the tool blocks a Type B comparison instead of substituting zero or the listed volume.
The TS-30 table lists work-bowl volume and3,000rpm. Keep the two-factor drive-power notation as printed. A drive-power sum or operating-energy estimate is not produced. The2023brochure includes R500/1500, which this factsheet omits; its current availability is not established.
Compare with your own catalog limits
Choose a listed volume basis. Leave all four limit inputs blank for the catalog comparison, or enter all four positive decimal values to screen the listed values. No limits are prefilled. Dimensions remain catalog fields; obtain the supplier installation drawing and loading guidance.
Separate work-bowl and machine geometry
A bowl width is 500 versus 500 mm, B bowl height 580 versus 580 mm, and C bowl length 800 versus 1000 mm.
Complete-machine D/E/F dimensions are 2355/715/1130 mm for R 500/800 and 2590/715/1020 mm for R 500/1000. The tool screens these three listed dimensions against your own maximum values; it does not include service, guarding, utility or loading allowances.
The work-bowl shape and lining matter. Do not multiply A, B and C into a rectangular capacity or infer permissible part fit. Record workpiece geometry, material, sensitivity, fixturing and media flow; confirm permissible loading and trial conditions with the manufacturer. None of these catalog values provides a cycle time, media recipe, batch weight or parts-per-hour figure.
Read the drive fields on their source basis
Drive power is printed as 2 x 4,0 versus 2 x 4,0 kW. The multiplication notation is retained. No scalar power difference, motor-total or consumption estimate is calculated.
Both rows are under the 3000 rpm drive-speed heading. The table states no electrical frequency for that heading. It is not a recommended process speed.
Source: Roesler Tub Vibrators factsheet, physical page 2, revision 05/2024. The same PDF has other page revisions: pages1/3 use04/2023, page2 uses05/2024. This pair uses the revision printed on its table page. The EN.129.21 revision04/2023 brochure provides additional family context; it is the same publisher, not an independent measurement.
Confirm current offered configuration, availability, utilities, floor loading, service access and guarding with the manufacturer. No manufacturer partnership, current build or Jintaijin equivalence is established.
Questions about this pair
What changes between R 500/800 and R 500/1000 in TS-30?
The TS-30 table lists 210 L for R 500/800 and 260 L for R 500/1000, a right-minus-left difference of 50 L. The basis is work-bowl volume (profile not specified in volume column). These values are not permissible part loads, batch weights or throughput. Type B volume is not listed for both models; the tool blocks a Type B comparison instead of substituting zero or the listed volume. Complete-machine D/E/F dimensions are 2355/715/1130 mm for R 500/800 and 2590/715/1020 mm for R 500/1000. The tool screens these three listed dimensions against your own maximum values; it does not include service, guarding, utility or loading allowances.
Can Type B volume be used for this pair?
No. Both source rows do not provide a Type B volume. A missing value is unknown, not zero and not an equivalent of the listed volume. The tool disables the Type B selection and rejects a forced unsupported comparison.
Do the drive values establish process speed or consumption?
Drive power is printed as 2 x 4,0 versus 2 x 4,0 kW. The multiplication notation is retained. No scalar power difference, motor-total or consumption estimate is calculated. Both rows are under the 3000 rpm drive-speed heading. The table states no electrical frequency for that heading. It is not a recommended process speed.
What does a passing four-limit screen mean?
It means the selected listed volume meets your minimum and the listed D/E/F complete-machine dimensions meet your three maxima. Enter all four positive decimal limits or leave all four blank. A passing screen is not workpiece-fit, permissible loading, installation, electrical or process approval. Confirm current configuration, drawings and trial conditions with the manufacturer; no Jintaijin equivalence is established.
Related trial and inspection tools
Discuss your workpiece and sample-trial requirements with Jintaijin