Jintaijin | Independent versioned catalog reference

Roesler Z 1000 ASS-II-Turbo vs Z 800 HA Turbo-Floc: liquid-cleaning catalog comparison

Compare Z 1000 ASS-II-Turbo and Z 800 HA Turbo-Floc using the Roesler centrifuge factsheet, physical page 2, revision 07/2024. Keep liquid flow, sludge volume or mass, power and options on their printed basis. Filter the fields, enter your own liquid-flow requirement and optional solids concentration, and export the current review record. Confirm actual cleaning performance and the offered configuration through supplier drawings and a representative fluid trial.

Roesler Z 1000 ASS-II-Turbo vs Z 800 HA Turbo-Floc: liquid-cleaning catalog comparison - liquid-flow diagram - Jintaijin
Original liquid flow data diagram for this model pair; factsheet page 2, revision07/2024.

Read each source field on its own basis

Field groupZ 1000 ASS-II-TurboZ 800 HA Turbo-Floc
SpeedMax. rotational speed (RPM)
2,770 RPM
Max. rotational speed (RPM)
2,930 RPM
ForceMax. “g” value
2,000 g
Max. “g” value
1,750 g
Sludge volumeMax. sludge volume (l)
28 l
Max. sludge volume (l)
11 l
Sludge massDrum capacity (kg)
30 kg
basket capacity (kg)
28 kg
FlowCapacity 1 (l/h)
800 - 3,500 2 l/h
Capacity1 (l/h)
1,200 l/h
InstalledInstalled power (kW)
11 kW
Installed power (kW)
5.0 kW
AverageAverage power draw (kW) 3
6.5 kW
Average power draw (kW)
2.2 kW
Dirty tankDirty water tank (l) optional 3
700/1,000/2,000 l
Dirty water tank (l)
250 l
Clean tankClean water tank (l) optional
700/1,000/2,000 l
Clean water tank (l)
- l
CoolingCooling of the process water
Option
Cooling of the process water
-
DosingAutomatic water and compound replenishment dosing system
Option
Automatic water and compound replenishment dosing system
optional

The printed liquid-flow entry is 800 - 3,500 2 l/h for Z 1000 ASS-II-Turbo and 1,200 l/h for Z 800 HA Turbo-Floc. These process-water entries are in litres per hour and depend on solids load and the desired cleaning effect. The Z1000 range and its separate lower-solids-load footnote are retained without selecting an operating rate. Tank configuration and sludge handling require separate review.

Review source fields and your fluid inputs

Choose a field group. Flow is optional; solids concentration requires flow. No process values are prefilled. Catalog comparisons do not select a centrifuge or prove the desired cleaning effect.

Compare the source fields, or enter your own flow and optional solids concentration.
Roesler Z 1000 ASS-II-Turbo vs Z 800 HA Turbo-Floc: liquid-cleaning catalog comparison - sludge-basis diagram - Jintaijin
Original sludge basis data diagram for this model pair; factsheet page 2, revision07/2024.

Separate fluid load from collected sludge

Z 1000 ASS-II-Turbo: Max. sludge volume (l) = 28 l, Drum capacity (kg) = 30 kg; Z 800 HA Turbo-Floc: Max. sludge volume (l) = 11 l, basket capacity (kg) = 28 kg. Volume and mass are separate source bases. A range does not select a basket insert, and a volume does not establish a sludge mass without density and loading evidence.

The optional incoming-solids calculation uses your own flow and concentration. It does not infer captured solids, residual moisture, sludge density, cake volume or basket-fill duration. Ask the supplier to establish these quantities with the actual liquid and an agreed cleaning target before selecting a discharge or handling schedule.

Record liquid composition, temperature, solids concentration, particle-size distribution, material densities, emulsified or free oil and the desired cleaning effect. Also record variability during a shift, collection and return paths, tank arrangements and sample handling. A nominal maximum flow cannot replace this fluid-specific review.

Roesler Z 1000 ASS-II-Turbo vs Z 800 HA Turbo-Floc: liquid-cleaning catalog comparison - power-basis diagram - Jintaijin
Original power basis data diagram for this model pair; factsheet page 2, revision07/2024.

Prepare a source-backed supplier review

Z 1000 ASS-II-Turbo: Installed power (kW) = 11 kW, Average power draw (kW) 3 = 6.5 kW; Z 800 HA Turbo-Floc: Installed power (kW) = 5.0 kW, Average power draw (kW) = 2.2 kW. Original options and catalog averages remain visible; this tool does not turn them into measured electricity use for your process.

Request an offered configuration with current electrical, tank, cooling, dosing, sludge-removal and access details. Specify how inlet and outlet samples will be collected and how the required cleaning effect will be measured. Obtain a trial result rather than adopting a catalog capacity as guaranteed performance. No installation dimensions or floor-loading approval is supplied by the selected tables.

Source: Roesler centrifuge factsheet, physical page 2, revision07/2024. Industrial-liquid cleaning centrifuge brochure supplies RZ context. RZ120M-3PH has conflicting official flow entries and is excluded from this tool.

This independent catalog reference does not establish current availability, Jintaijin equipment equivalence or manufacturer partnership.

Questions about this pair

How do Z 1000 ASS-II-Turbo and Z 800 HA Turbo-Floc differ in catalog liquid flow?

The printed liquid-flow entry is 800 - 3,500 2 l/h for Z 1000 ASS-II-Turbo and 1,200 l/h for Z 800 HA Turbo-Floc. These process-water entries are in litres per hour and depend on solids load and the desired cleaning effect. The Z1000 range and its separate lower-solids-load footnote are retained without selecting an operating rate. Tank configuration and sludge handling require separate review.

Can the sludge entries be used to set an emptying interval?

Z 1000 ASS-II-Turbo: Max. sludge volume (l) = 28 l, Drum capacity (kg) = 30 kg; Z 800 HA Turbo-Floc: Max. sludge volume (l) = 11 l, basket capacity (kg) = 28 kg. Volume and mass are separate source bases. A range does not select a basket insert, and a volume does not establish a sludge mass without density and loading evidence. No. Incoming solids, captured solids and wet cake are different quantities. Density, capture efficiency, cake moisture, usable capacity and loading pattern would need separate evidence.

Do the power entries predict operating cost?

Z 1000 ASS-II-Turbo: Installed power (kW) = 11 kW, Average power draw (kW) 3 = 6.5 kW; Z 800 HA Turbo-Floc: Installed power (kW) = 5.0 kW, Average power draw (kW) = 2.2 kW. Original options and catalog averages remain visible; this tool does not turn them into measured electricity use for your process. No current duty cycle, fluid-specific trial or energy measurement protocol is established by this record.

What does the interactive flow and solids review calculate?

The tool converts your flow input between l/min and l/h and, when you also enter solids concentration in g/l, computes incoming solids in kg/h as flow_l/h × concentration_g/l ÷ 1000. It compares your flow only against a scalar printed catalog reference; ranges keep a no-value-selected status. At or below a reference is not approval of cleaning performance. The computed solids are your input mass balance, not captured sludge, part throughput or an emptying schedule. Export uses the current field group and inputs.

Related trial and inspection tools

Discuss your workpiece and fluid-trial requirements with Jintaijin

Prepare a high-appearance machinery review

Use this local checker to identify missing part and inspection information. It prepares a technical-review brief; it does not approve a machine, process recipe or production result.

Complete the part details to prepare a review brief.

Open the enquiry form for this page

Plan batch capacity from trial measurements

#+86-592-2381506

Email : info@surface-polish.com

Headquarters address : No. 31, Xinchang Road, Xinyang Industrial Zone, Haicang District, Xiamen

click here to leave a message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Preparing secure enquiry form…

Home

Products

whatsapp

contact