Jintaijin | Independent specification reference
Walther Trowal CB 200 vs CB 300: specification comparison
Compare CB 200 and CB 300 in the CB circular vibratory finishing machines official table. Gross volume is 200 versus 300 L; maximum drive power at 1,500 rpm is 4 versus 4 kW. Use the tool to inspect differences, enter your own gross-volume and listed-power limits, and download the current comparison. Conditional volume figures need a workpiece-specific review.
Listed specification differences
| Source field | CB 200 | CB 300 | Right minus left |
|---|---|---|---|
| Gross bowl volume | 200 L | 300 L | 100 L |
| Conditional useful volume | 125 L | 190 L | 65 L |
| Listed maximum workpiece dimension | 170 mm | 220 mm | 50 mm |
| Screen area | 2190 cm² | 2710 cm² | 520 cm² |
| Empty weight | 740 kg | 935 kg | 195 kg |
| Maximum drive power at 1,500 rpm | 4 kW | 4 kW | 0 kW |
| Maximum centrifugal force | 49000 N | 49000 N | 0 N |
Gross volume increases by 100 L, from 200 to 300 L. The table lists 125 L conditional useful volume for CB 200 and 190 L conditional useful volume for CB 300. These are conditioned by workpiece geometry, material, sensitivity and the media-to-parts ratio; they do not guarantee a batch of parts.
Maximum drive power at 1,500 rpm changes from 4 to 4 kW, a difference of 0 kW. Screen area changes from 2190 to 2710 cm²; empty weight from 740 to 935 kg. The listed maximum workpiece dimension is 170 versus 220 mm, which alone does not approve a particular part.
Compare with your own catalog limits
Leave both inputs blank to compare the listed values. Enter both limits to include an arithmetic screen. No limit is prefilled. The power field used here is maximum drive power at 1,500 rpm.
Read the volume condition before planning a batch
Gross volume increases by 100 L, from 200 to 300 L. The table lists 125 L conditional useful volume for CB 200 and 190 L conditional useful volume for CB 300. These are conditioned by workpiece geometry, material, sensitivity and the media-to-parts ratio; they do not guarantee a batch of parts.
Parts and media occupy the working mixture together. Do not convert the conditional figure or its endpoints into parts per hour, guaranteed batch weight, packing fraction or a media recipe. Record part geometry, material and sensitivity, then confirm the permissible loading and separation conditions with the supplier and a workpiece-specific trial.
Drive values and source basis
Maximum drive power at 1,500 rpm changes from 4 to 4 kW, a difference of 0 kW. Screen area changes from 2190 to 2710 cm²; empty weight from 740 to 935 kg. The listed maximum workpiece dimension is 170 versus 220 mm, which alone does not approve a particular part.
The official Walther Trowal CB circular vibratory finishing machines table was captured on 2026-10-04. No manufacturer revision is stated on the HTML table. Listed power is not measured energy use or an estimate of operating cost. Lettered drawing dimensions are not converted to a floor-space rectangle. Obtain current drawings for guarding, service access, utilities and floor loading.
These are independent source references. No manufacturer partnership, current configuration, availability or Jintaijin equivalence is established.
Questions about this pair
What changes between CB 200 and CB 300?
Gross volume increases by 100 L, from 200 to 300 L. The table lists 125 L conditional useful volume for CB 200 and 190 L conditional useful volume for CB 300. These are conditioned by workpiece geometry, material, sensitivity and the media-to-parts ratio; they do not guarantee a batch of parts. Maximum drive power at 1,500 rpm changes from 4 to 4 kW, a difference of 0 kW. Screen area changes from 2190 to 2710 cm²; empty weight from 740 to 935 kg. The listed maximum workpiece dimension is 170 versus 220 mm, which alone does not approve a particular part.
Does the useful or net volume guarantee a batch of parts?
No. The source conditions the figure on workpiece geometry, material and sensitivity, which determine the media-to-parts ratio. Supplier review and a referenced trial are needed for permissible part load, handling and process conditions.
What do the two optional limits check?
The tool compares gross volume against your entered minimum and the listed power field against your entered maximum. Enter both positive decimal values or leave both blank. A passing arithmetic check is not part-fit, process, electrical, installation or throughput approval.
Are these current specifications or Jintaijin equivalents?
The source is an official HTML table captured on 2026-10-04, with no manufacturer revision stated. Confirm the actual offered configuration and availability with Walther Trowal. These facts do not describe a Jintaijin model or establish equivalence.
Related trial and inspection tools
Discuss your workpiece and sample-trial requirements with Jintaijin