Walther Trowal trowal AG 26 vs trowal LZ 11 pickling / ball-burnishing compound catalog comparison
Review trowal AG 26 and trowal LZ 11 from the official Pickling and ball-burnishing liquids brochure marked 01/22, physical PDF page 13. Compare 6 source fields, retaining units, qualitative symbols and conditional bases. This pair differs in 6 adopted fields. Record your sample objective, compatibility or loading questions, safety and site requirements, and acceptance method. The comparison download uses your current form entries.
Compare source rows and record review questions
Versioned catalog rows
| Source field | trowal AG 26 | trowal LZ 11 |
|---|---|---|
| Descriptive pH label | Acidic | Highly acidic |
| Pickling symbol | + | ++ |
| Cleaning symbol | ++ | 0 |
| Degreasing symbol | ++ | 0 |
| Foaming wording | Extensive foaming | Minor foaming |
| Printed remark | Finishing of silver | Finishing of copper and brass |
Properties entries for this pair
Descriptive pH label: trowal AG 26 Acidic; trowal LZ 11 Highly acidic.
Characteristics entries for this pair
Pickling symbol: trowal AG 26 +; trowal LZ 11 ++. Cleaning symbol: trowal AG 26 ++; trowal LZ 11 0. Degreasing symbol: trowal AG 26 ++; trowal LZ 11 0.
Remarks entries for this pair
Foaming wording: trowal AG 26 Extensive foaming; trowal LZ 11 Minor foaming. Printed remark: trowal AG 26 Finishing of silver; trowal LZ 11 Finishing of copper and brass.
Source reading and conditions
Publisher qualitative legend: ++ very good suitability; + good suitability; 0 limited suitability; - no suitability. These categories are not measured values or percentages. Blank remarks are NOT_LISTED. Paste footnote markers remain visible; *) states cycle time more than 24 hours. A merged remark is marked SHARED_REMARK_NOT_INDEPENDENTLY_MAPPED.
- Publisher symbols ++, +, 0 and - are qualitative categories, never numeric scores or measured performance. Blank remarks are NOT_LISTED, not the printed minus symbol.
- A descriptive pH label is not a numeric pH range. No dilution, mixing, dosing recipe, SDS, part approval or current offer is established.
- The source is an independent Walther Trowal reference, not proof of Jintaijin supply, equivalence, partnership or a customer trial.
- Source application remarks do not establish a surface finish or compatibility with a specific alloy. No pickling recipe is provided.
Source and sample-review scope
Official Pickling and ball-burnishing liquids brochure, 01/22, physical page 13, captured 2026-10-05.
Use this independent Walther Trowal reference to prepare a supplier and sample discussion. It does not establish Jintaijin supply, partnership, an equivalent product, current offers or a customer trial. Obtain a current specification and safety documentation, then define a real sample, part or liquid-stream objective, constraints and acceptance method. User annotations remain USER_RECORDED_NOT_VERIFIED. No mixing, dosing, compatibility, hygiene or wastewater-discharge approval follows from this page.
Questions about this pair
Which adopted fields differ for trowal AG 26 and trowal LZ 11?
Descriptive pH label: trowal AG 26 Acidic versus trowal LZ 11 Highly acidic. Pickling symbol: trowal AG 26 + versus trowal LZ 11 ++. Cleaning symbol: trowal AG 26 ++ versus trowal LZ 11 0. Degreasing symbol: trowal AG 26 ++ versus trowal LZ 11 0. Foaming wording: trowal AG 26 Extensive foaming versus trowal LZ 11 Minor foaming. Printed remark: trowal AG 26 Finishing of silver versus trowal LZ 11 Finishing of copper and brass.
How should source symbols and missing remarks be read?
Publisher qualitative legend: ++ very good suitability; + good suitability; 0 limited suitability; - no suitability. These categories are not measured values or percentages. Blank remarks are NOT_LISTED. Paste footnote markers remain visible; *) states cycle time more than 24 hours. A merged remark is marked SHARED_REMARK_NOT_INDEPENDENTLY_MAPPED.
What source conditions must remain visible?
Publisher symbols ++, +, 0 and - are qualitative categories, never numeric scores or measured performance. Blank remarks are NOT_LISTED, not the printed minus symbol. A descriptive pH label is not a numeric pH range. No dilution, mixing, dosing recipe, SDS, part approval or current offer is established. The source is an independent Walther Trowal reference, not proof of Jintaijin supply, equivalence, partnership or a customer trial. Source application remarks do not establish a surface finish or compatibility with a specific alloy. No pickling recipe is provided.
Can these entries predict a process result or cost?
Versioned catalog values and symbols retain their source row bases; they are not measured trials or approved process settings. Symbols ++, +, 0 and - are qualitative; no numeric score, ranking or dosage is calculated. Descriptive pH is not a numeric range; media fill, batch volume and mass retain separate meanings. No part compatibility, finish, hygiene, discharge compliance, installed configuration or current offer is established. Independent Walther Trowal reference; Jintaijin supply, partnership and equivalence are not established. User annotations are not verified trials or customer facts.
What must the current supplier and sample review establish?
Use this independent Walther Trowal reference to prepare a supplier and sample discussion. It does not establish Jintaijin supply, partnership, an equivalent product, current offers or a customer trial. Obtain a current specification and safety documentation, then define a real sample, part or liquid-stream objective, constraints and acceptance method. User annotations remain USER_RECORDED_NOT_VERIFIED. No mixing, dosing, compatibility, hygiene or wastewater-discharge approval follows from this page.
Related review tools
Prepare a sample-review enquiry
Provide a drawing or liquid-stream description, objective, constraints and acceptance method for a SurfacePolish discussion.
Open the SurfacePolish enquiry form