Polishing Metal with JintaiJin Vibration Machine: A Step-by-Step Guide Mar 13, 2023
Tableware knife and fork polishing
Polishing Metal with JintaiJin Vibration Machine: A Step-by-Step Guid

JintaiJin vibration grinding and polishing machine is a powerful tool that can be used to polish the surface of metal products. This machine uses a high-speed vibration to remove the roughness and scratches from the surface of the metal and give it a smooth and polished finish. In this article, we will discuss how to use JintaiJin vibration grinding and polishing machine to polish the surface of metal products, and also provide a video showcasing the polishing effect on hairdressing scissors.

Step 1: Clean the Metal Surface
Before starting the polishing process, it is important to clean the metal surface thoroughly. Any dirt or debris on the surface can cause scratches or damage to the metal during the polishing process. Use a soft cloth and a cleaning solution to wipe the surface of the metal and remove any dirt, dust or grease.

Step 2: Select the Right Polishing Media
Selecting the right polishing media is crucial for achieving the desired result. The type of media you use will depend on the type of metal and the level of finish you want to achieve. Some of the most commonly used polishing media include ceramic, plastic, and steel.

Step 3: Set Up the Machine
Place the metal product to be polished in the JintaiJin vibration grinding and polishing machine. Ensure that the product is securely held in place and will not move or slip during the polishing process. Add the polishing media to the machine, making sure not to overload it. You want to ensure that there is enough space for the media to move around and polish the surface of the metal evenly.

Step 4: Start the Machine
Once the machine is set up, switch it on and adjust the speed and time settings according to the type of metal and the level of finish you want to achieve. The vibration and motion of the media will create friction on the metal surface, which will gradually polish it and remove any roughness or scratches.

Step 5: Monitor the Polishing Process
Monitor the polishing process closely to ensure that the metal surface is polished evenly and consistently. Check the progress periodically and adjust the speed and time settings if necessary. Once you have achieved the desired level of finish, switch off the machine and remove the metal product.

Video showcasing the polishing effect on hairdressing scissors:

Hairdressing scissors are a common tool used in the hairdressing industry. They require regular maintenance to ensure that they remain sharp and effective. JintaiJin vibration grinding and polishing machine can be used to polish the surface of hairdressing scissors, giving them a polished and professional finish.

The following video demonstrates how to use JintaiJin vibration grinding and polishing machine to polish hairdressing scissors:


In conclusion, JintaiJin vibration grinding and polishing machine is an effective tool for polishing the surface of metal products. By following the steps outlined above, you can achieve a smooth and polished finish on your metal products. Additionally, the video showcasing the polishing effect on hairdressing scissors demonstrates how JintaiJin vibration grinding and polishing machine can be used to Surface treatment on metal products
StepWhat to establishWhy
Define the targetWhat the surface must reach and what must be preservedSets the limit the process works within
Choose mediaShape and size from the smallest featureMedia that cannot enter cannot work the feature
Set the loadPart-to-media ratio for the actual partsOverloading shields parts instead of working them
Set compound and waterConcentration and flow for the materialFines build up and weaken the action without flow
Run a sampleConfirm the result on representative partsA full batch is not the place to find out
Record the outcomeMedia, compound, cycle, load and observationsMakes the result repeatable

Directions to test on a representative sample, not validated results for a specific component.

#+86-592-2381506

Email : info@surface-polish.com

Headquarters address : No. 31, Xinchang Road, Xinyang Industrial Zone, Haicang District, Xiamen

click here to leave a message