Query six current flat magnetic finishing model records using a minimum published workpiece capacity and three maximum outside dimensions. The result is a match to stated table fields, not a recommendation to run the entered weight. Keep the working-area dimensions, part geometry, circulation and separation evidence with the equipment comparison.

Compare the published family fields

Enter comparison fields from this equipment family.

OBD-30

Published workpiece capacity (kg)
30.0
Processing area (mm)
1000 × 580
Outside L × W × H (mm)
1300 × 850 × 750
Net machine weight (kg)
350.0
Motor rating (kW)
4.0
Published speed expression
0-1800

OBD-35

Published workpiece capacity (kg)
35.0
Processing area (mm)
1080 × 680
Outside L × W × H (mm)
1300 × 850 × 750
Net machine weight (kg)
350.0
Motor rating (kW)
5.5
Published speed expression
0-1800

OBD-60

Published workpiece capacity (kg)
60.0
Processing area (mm)
1800 × 580
Outside L × W × H (mm)
2000 × 850 × 750
Net machine weight (kg)
600.0
Motor rating (kW)
6.0
Published speed expression
0-1800

OBD-70

Published workpiece capacity (kg)
70.0
Processing area (mm)
1900 × 680
Outside L × W × H (mm)
2000 × 850 × 750
Net machine weight (kg)
600.0
Motor rating (kW)
11.0
Published speed expression
0-1800

OBD-90

Published workpiece capacity (kg)
90.0
Processing area (mm)
2200 × 580
Outside L × W × H (mm)
2500 × 850 × 750
Net machine weight (kg)
800.0
Motor rating (kW)
12.0
Published speed expression
0-1800

OBD-100

Published workpiece capacity (kg)
100.0
Processing area (mm)
2300 × 680
Outside L × W × H (mm)
2500 × 850 × 750
Net machine weight (kg)
800.0
Motor rating (kW)
16.5
Published speed expression
0-1800

Six records, one family comparison

The OBD-30 and OBD-100 primary pages carry the same six-column specification table. The query consolidates that repeated family information rather than creating a separate page for each source URL. Published workpiece capacities are 30, 35, 60, 70, 90 and 100 kg. These labels are reference ratings; a particular part load must still be checked in a representative trial.

Outside size does not equal processing area

OBD-30 and OBD-35 share a 1300 × 850 × 750 mm outside envelope, while their listed processing areas differ. OBD-60/70 and OBD-90/100 also share outside-envelope pairs. A model passing the external-size filter therefore does not establish that a particular drawing fits the active working area or receives the intended motion. Read the area record separately and obtain the current layout drawing.

How the four filters combine

A record remains visible only when published capacity is at least the entered minimum and each published outside axis is no greater than its matching maximum. Equal boundary values are included. Enter length, width and height in the published axis order; do not rotate them silently to obtain a match. The input maxima describe comparison limits and do not reserve operator or service clearance.

Why not rank by motor power?

The source has different motor ratings across the family even when two models share an outside envelope. The query preserves those ratings but does not rank polishing quality, throughput or energy consumption from them. A drive nameplate value is not a measured average demand, and a larger published rating does not establish that a protected edge will remain acceptable.

What should a part trial record include?

Identify the material, incoming burr, feature access, contact-sensitive areas and the target inspection method. Keep the actual load, media identity, settings and observed separation result with the record. Check both the intended finish and protected-feature condition before treating the equipment match as a production decision. No generic magnetic finishing cycle or compound concentration is selected here.

Flat magnetic finishing six-model parameter query - Published workpiece capacity, not validated loading - Jintaijin
Published workpiece capacity, not validated loading. Reference fields and review method; no trial outcome is claimed.
Flat magnetic finishing six-model parameter query - Shared external envelopes do not prove equal working area - Jintaijin
Shared external envelopes do not prove equal working area. Reference fields and review method; no trial outcome is claimed.
Flat magnetic finishing six-model parameter query - From table comparison to representative trial - Jintaijin
From table comparison to representative trial. Reference fields and review method; no trial outcome is claimed.

Related equipment and production reviews

Source and technical review

Source tables checked 3 October 2026: Primary model table 1 · Primary model table 2. Published reference fields require confirmation for the supplied build and the intended part trial.

Open the enquiry form with this family reference. Filtering stays in this page and does not submit an enquiry.

Review the part conditions alongside machine dimensions

A capacity or outside-dimension match does not settle retained-pin, deformation or acceptance risks. Combine all relevant part conditions in the trial plan before requesting a machine review.

Magnetic finishing part-condition inspection planner

Compare exact magnetic-flat model pairs

Compare the published differences in capacity, processing area, outer envelope and motor rating; each page starts with a specific pair. Current supplied configuration and usable part loading still require confirmation.

#+86-592-2381506

Email : info@surface-polish.com

Headquarters address : No. 31, Xinchang Road, Xinyang Industrial Zone, Haicang District, Xiamen

click here to leave a message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Preparing secure enquiry form…

Home

Products

whatsapp

contact