Compare three large tub-vibrator models using the current published technical table. Enter a minimum nominal capacity and maximum outside length, width and height to show records that meet all four numeric filters. Review model-specific motor expressions, net weights and divider notes alongside the filtered result. The query does not establish part fit, usable loading, installation clearance or accepted production output.
Enter your comparison limits, then filter the source table.
The source identifies L1300 at 1200 L, L1500 at 1500 L and L1800 at 1800 L. The L1300 name is therefore not a 1300-liter specification. Filter by the capacity field rather than the digits in the model label. Nominal liters do not define the amount of parts that can circulate with the selected media.
The table expressly labels outside dimensions as length × width × height. L1300 is 2700 × 1300 × 1400 mm, L1500 is 3340 × 1290 × 1440 mm and L1800 is 2800 × 1700 × 2000 mm. The length ordering is not the capacity ordering: do not extrapolate an intermediate model size from liters alone. The filter applies each axis independently and includes values equal to your entered limit.
A match means only that the reviewed published nominal capacity is at least your capacity filter and all three published outside dimensions are no greater than the entered axis limits. These limits are comparison criteria, not required safe access distances. Add independently confirmed installation, handling and service needs before approving a room layout. A model disappearing from the list does not prove that a customized build is unavailable.
The source also provides working-bowl dimensions. They remain dimensional references rather than a rectangular usable-volume calculation. Actual chamber shape, liners, dividers, media loading and circulation affect the trial. Confirm the current chamber drawing and permitted loading for your part. This query uses neither a part density nor a time-to-finish coefficient and cannot choose a media recipe.
The motor terms are preserved as 5.0 kW × 2, 5.5 kW × 2 and 7.5 kW × 2 for the three respective models. They describe the source configuration, not measured electrical demand or cycle energy. Obtain the supplied electrical specification and measured duty conditions before using power figures in a cost model.
The table marks chamber divider availability as an optional accessory for all three models. Availability does not establish the number, spacing, isolation performance or price of an installed divider set. State which contact-sensitive surfaces and loading groups the trial must protect, then confirm the actual divider arrangement.
Save the model names that match your comparison criteria. Send the part drawing, material, starting condition, protected features, target finish, intended loading and separation route. Include the needed handling envelope and utility details. Ask for the current model drawing and supplied configuration. Keep a published-table match separate from a passed part trial and final acceptance evidence.
Each equipment family keeps its own capacity units and technical fields. Use the corresponding source records when your review also includes magnetic finishing, drying or dry tumbling.
Source table checked 3 October 2026: Jintaijin large tub-vibrator model range. Values describe a published reference configuration. Confirm the actual supplied build.
Open the enquiry form with this model-query reference. Filtering does not send an enquiry.
Keep motor count and each identical motor rating separate from their arithmetic sum when reviewing a supplier quote.
Compare the quoted motor count and individual rated kW with the published tub configuration
Compare published nominal liters, internal chambers, outer envelopes, net weights and dual-motor ratings. No usable load or accepted output is inferred.
Email : info@surface-polish.com